Excess moisture beneath flooring can trigger widespread failures, from bubbling adhesives to warped timber, says Richard Renouf. Understanding the causes, effects and testing methods is essential
HIGH moisture levels in a subfloor are responsible for a lot of flooring failures. Typical moisture issues that affect flooring include screeds that have not been allowed to fully dry before laying flooring and subfloors in older properties (typically those built before 1970) where there is no damp-proof membrane between the earth and the floor slab to protect from ground moisture.
Resilient flooring of all kinds will trap excess subfloor moisture and prevent it escaping to the atmosphere. The trapped moisture causes adhesives to soften so the flooring will then blister and bubble as the adhesive bond breaks down. Some other subfloor preparation products, such as smoothing compounds, are not moisture tolerant and so can also fail, sometimes before the adhesive is affected.
This can result in the compound delaminating from the screed causing a crackling noise underfoot, and sometimes visible unevenness under the flooring. Such failures are often accompanied by the splitting of welds on sheet flooring and gapping on LVT products.
Wood absorbs moisture from its surroundings until it reaches equilibrium – the point where the moisture in the wood is stable. As it takes on moisture it will expand and when it releases moisture it will contract, and fitting methods take this natural movement into account so that the normal fluctuations in atmospheric moisture do not cause problems.
Where there’s excessive moisture in the subfloor, the wood will absorb moisture, so solid and engineered wood flooring will expand and this will often cause warping and lifting from the subfloor. Wood warps because it expands and shrinks much more around the circumference (along the growth rings you see on the end grain of a piece of wood) than it does at right angles to them.
Depending on how the wood has been cut from the log, the wood may cup, crown or twist. On engineered wood floors which have strips of wood at the core, this can even result in the floor surface looking rippled because the individual strips have warped.
Floating floors, such as laminate and SPC, are also affected by moisture. Laminate flooring will cup if it’s protected by a moisture barrier when laid on a subfloor with high moisture as the back of the planks swells slightly, causing them to curl. This also happens for SPC flooring which has a waterproof surface but has mineral fillers (usually limestone – a porous mineral that dissolves in water, causing scale in many areas of the UK) which absorb the moisture and cause cupping. When wetted on the surface, the joints of laminate flooring allow moisture in and this then is absorbed sideways into the planks causing uneven swelling along the joint lines.
It is usually quite obvious when moisture has caused a problem, but that is not the full story and a flooring inspector should carry out further investigation and testing to establish the source of the moisture. This will confirm the reason for the failure and will also enable a solution to be worked out so that the problem does not recur when remedial work is done. This is just as important if the moisture has dried down to an acceptable level by the time of the inspection, because it will then be clear whether the moisture could build up again or is no longer a threat to the flooring.
Moisture testing is usually easiest when carried out before flooring is laid and there have been many articles in CFJ about the methods of testing available to a flooring contractor.
British Standards, and manufacturers’ guidelines place a clear responsibility on a flooring contractor to ensure a subfloor has been tested to ensure the moisture levels are at or below the required level (usually stated as 75% RH or 65% RH for some flooring and/or over underfloor heating) but the amount of floor failures I see shows this is not always done, or measuring instruments are not checked or are cheap and not up to job.
One reason for this may be that the British Standard method for moisture testing is the hygrometer box. This measures the relative humidity of air above the floor surface and so give a relative humidity (RH) reading directly comparable to the BS requirements. However, it takes at least two days and usually a bit longer, so it’s not practical when you’re inspecting a failed floor and cannot get back to site to take the readings. There are, however, ways to get indicative readings straight away and in next month’s article we’ll consider what an inspector can do to get the needed information and to check that it’s accurate.
www.richard-renouf.com